产品代码 : 3D-Superalloy-CU-PO1
A superalloy is a kind of metal material based on iron, nickel, and cobalt, which can work at high temperatures above 600℃ and under certain stress for a long time. It has excellent high-temperature strength, good oxidation resistance and thermal corrosion resistance, good fatigue performance, fracture toughness, and other comprehensive properties, and is also known as "superalloy". Spherical Superalloy Powder is usually used in 3D printing.
如果您需要定制服务,请联系我们。 我们将在 24 小时内与您联系并告知价格和可用性。
| 产品 | 产品代码 | 纯度 | 尺寸 | 联系我们 |
Spherical Superalloy Powder Particle Size
0-15μm, 5-25μm, 15-45μm, 15-53μm, 45-75μm, 45-105μm, 75-150μm. (Various granularities can be customized according to customer requirements)
Spherical Superalloy Powder Grade
| Grade | Chemical Composition | Particle Size Distribution | |
| Elements | Inpurities | ||
| IN625(GH3625) | Cr: 20.0-23.0 Mo: 8.0-10.0 Nb: 3.15-4.15 Fe: ≤5.0 Si: ≤0.50 Ni: Bal | Ti: ≤0.40 Al: ≤0.40 C: ≤0.10 Co: ≤1.00 S: ≤0.015 P: ≤0.015 Y: ≤0.005 | 15-45μm 15-53μm 53-120μm 53-150μm |
| IN718(GH4169) | Ni: 50.0-55.0 Cr: 17.0-21.0 Nb: 4.75-5.25 Mo: 2.80-3.30 Ti: 0.65-1.15 Al: 0.20-0.80 Cu: ≤0.30 Ni: Bal | O: ≤0.01 | 15-45μm 15-53μm 53-120μm 53-150μm |
| IN713(K418) | Cr: 11.5-13.5 Mo: 3.8-4.8 Al: 5.5-6.4 Ti: 0.5-1.0 Nb: 1.8-2.5 N: Bal | C: 0.08-0.16 Fe: ≤1.0 O: ≤0.01 | 15-45μm 15-53μm 53-120μm 53-150μm |
| IN939 | Cr: 22.0-22.8 Co: 18.5-19.5 W: 1.8-2.2 Nb: 1.8-2.5 Ta: 1.3-1.5 Ti: 3.6-3.8 Al: 1.8-2.0 Zr: 0.05-1.4 Ni: Bal | C: 0.13-0.17 B: 0.004-0.012 N: ≤0.001 S: ≤0.001 Pb: ≤0.001 Bi: ≤0.001 Ag: ≤0.001 O: ≤0.01 | 15-45μm 15-53μm 53-120μm 53-150μm |
| IN738LC | Cr: 14.0-16.0 Co: 8.0-9.00 Ti: 2.50-4.00 Al: 2.50-4.00 Mo: 1.00-2.00 W: 2.00-3.00 Ni: Bal | Ta: 1.00-2.00 Nb: 0.50-1.50 C: ≤0.15 Fe: ≤0.10 Zr: ≤0.10 B: ≤0.15 O: ≤0.01 | 15-45μm 15-53μm 53-120μm 53-150μm |
Spherical Superalloy Powder Particle Size Description
● 0-15μm (D10=3~5μm, D50=6~10μm, D90=12~14μm)
● 5-25μm (D10=5~10μm, D50=15~20μm, D90=20~25μm)
● 15-45μm (D10=15~20μm, D50=25~30μm, D90=35~40μm)
● 15-53μm (D10=15~20μm, D50=25~35μm, D90=45~50μm)
● 45-75μm (D10=45~55μm, D50=55~65μm, D90=70~75μm)
● 45-105μm (D10=50~60μm, D50=75~85μm, D90=95~105μm)
● 45-150μm (D10=55~70μm, D50=110~120μm, D90=140~150μm)
● 75-150μm (D10=80~90μm, D50=110~125μm, D90=135~150μm)


Spherical Superalloy Powder Application
Aerospace field, energy field
Spherical Superalloy Powder Applicable processes
Laser/electron beam additive manufacturing (SLM/EBM, 3D printing)
Direct laser deposition (DLD)
Powder hot isostatic pressing (HIP)
Metal injection molding (MIM)
Powder metallurgy (PM)
Laser cladding (LC), etc.
Packing of Spherical Superalloy Powder
Standard Packing:
Typical bulk packaging includes palletized plastic 5 gallon/25 kg. pails, fiber and steel drums to 1 ton super sacks in full container (FCL) or truck load (T/L) quantities. Research and sample quantities and hygroscopic, oxidizing or other air sensitive materials may be packaged under argon or vacuum. Solutions are packaged in polypropylene, plastic or glass jars up to palletized 440 gallon liquid totes Special package is available on request.
ATTs’Spherical Superalloy Powder is carefully handled to minimize damage during storage and transportation and to preserve the quality of our products in their original condition.